In early Chinese cast iron cannon production, which consequence occurs when the casting temperature is insufficient during a large pour?

A)Gas porosity weakens barrel integrity
B)Rapid cooling increases crystal size
C)Increased corrosion rates via oxidation
D)Metal segregates causing hard spots

💡 Explanation

Gas porosity arises because insufficient melt temperature prevents dissolved gasses from escaping during solidification; this forms voids via heterogeneous nucleation, therefore reducing the cannon's burst strength rather than improving its structural integrity or changing grain size.